Debye temperature of nanocrystalline Fe-Cr alloys obtained by mechanical alloying
Authors:
S. M. Dubiel,
B. F. O. Costa,
J. Cieslak,
A. C. Batista
Abstract:
A series on nanocrystalline Fe100-xCrx alloys prepared by mechanical alloying was investigated with X-ray diffraction (XRD), scanning electron microscopy (SEM) and Mössbauer spectroscopy (MS) techniques. XRD and SEM were used to structurally characterize the samples whereas MS permitted phase analysis as well as determination of the Debye temperature, Theta_D. Concerning the latter, an enhancement…
▽ More
A series on nanocrystalline Fe100-xCrx alloys prepared by mechanical alloying was investigated with X-ray diffraction (XRD), scanning electron microscopy (SEM) and Mössbauer spectroscopy (MS) techniques. XRD and SEM were used to structurally characterize the samples whereas MS permitted phase analysis as well as determination of the Debye temperature, Theta_D. Concerning the latter, an enhancement relative to bulk Theta_D-values was revealed in the range of ca. 40 < x <50. In a sample of Fe55.5Cr44.5 two phases were detected viz. (1) crystalline and magnetic with Theta_D=572(56) K and (2) amorphous and paramagnetic with Theta_D=405(26) K.
△ Less
Submitted 23 May, 2015;
originally announced May 2015.
-
On the Debye temperature in sigma-phase Fe-V alloys
Authors:
Jakub Cieslak,
Michael Reissner,
Stanislaw M. Dubiel,
Benilde F. O. Costa,
Walter Steiner
Abstract:
A series of sigma-phase Fe_{100-x}V_x samples with 34.4 < x < 59.0 were investigated by neutron and X-ray diffraction and Mossbauer spectroscopy (MS) techniques. The first two methods were used for verification of the transformation from alpha to sigma phase and they also permitted to determine lattice parameters of the unit cell. With MS the Debye temperature, T_D, was evaluated from the temper…
▽ More
A series of sigma-phase Fe_{100-x}V_x samples with 34.4 < x < 59.0 were investigated by neutron and X-ray diffraction and Mossbauer spectroscopy (MS) techniques. The first two methods were used for verification of the transformation from alpha to sigma phase and they also permitted to determine lattice parameters of the unit cell. With MS the Debye temperature, T_D, was evaluated from the temperature dependence of the centre shift, <CS>, assuming its entire temperature dependence originates from the second-order Doppler shift. To our best knowledge, it is the first ever-reported study on T_D in sigma-FeV alloys. Both attice parameters i.e. a and c were revealed to linearly increase with x. T_D shows, however, a non-monotonic behaviour as a function of composition with its extreme values between 425K for x=40 and 600K for x=59. A local maximum of 525K was found to exist at x=43.
△ Less
Submitted 3 March, 2010;
originally announced March 2010.
-
Debye temperature of disordered bcc-Fe-Cr alloys
Authors:
S. M. Dubiel,
J. Cieslak,
B. F. O. Costa
Abstract:
Debye temperature, TD, of Fe100-xCrx disordered alloys with 0<x<99.9 was determined from the temperature dependence of the centre shift of 57Fe Mossbauer spectra recorded in the temperature range of 80-300K. Its compositional dependence shows an interesting non-monotonous behaviour. For 0<x<~45 as well as for ~75<x<~95 the Debye temperature is enhanced relative to its value of a metallic iron, a…
▽ More
Debye temperature, TD, of Fe100-xCrx disordered alloys with 0<x<99.9 was determined from the temperature dependence of the centre shift of 57Fe Mossbauer spectra recorded in the temperature range of 80-300K. Its compositional dependence shows an interesting non-monotonous behaviour. For 0<x<~45 as well as for ~75<x<~95 the Debye temperature is enhanced relative to its value of a metallic iron, and at x=~3 there is a local maximum having a relative height of ~12% compared to a pure iron. For ~45<x<~75 and for x>~95 the Debye temperature is smaller than the one for the metallic iron, with a local minimum at x=~55 at which the relative decrease of TD amounts to ~12%. The first maximum coincides quite well with that found for the spin-waves stiffness coefficient, D0, while the pretty steep decrease observed for x>~95 which is indicative of a decoupling of the probe Fe atoms from the underlying chromium matrix is likely related to the spin-density waves which constitute the magnetic structure of chromium in that interval of composition. The harmonic force constant calculated from the Debye temperature of the least Fe-concentrated alloy (x>99.9) amounts to only 23% of the one characteristic of a pure chromium.
△ Less
Submitted 14 October, 2009;
originally announced October 2009.
-
Magnetic ordering above room temperature in the sigma-phase of Fe66V34
Authors:
Jakub Cieslak,
Benilde F. O. Costa,
Stanislaw M. Dubiel,
Michael Reissner,
Walter Steiner
Abstract:
Magnetic properties of four sigma-phase Fe_(100-x)V_x samples with 34.4<x<55.1 were investigated by Mossbauer spectroscopy and magnetic measurements in the temperature interval 5-300 K. Four magnetic quantities viz. hyperfine field, Curie temperature, magnetic moment and susceptibility were determined. The sample containing 34.4 at% V was revealed to exhibit the largest values found up to now fo…
▽ More
Magnetic properties of four sigma-phase Fe_(100-x)V_x samples with 34.4<x<55.1 were investigated by Mossbauer spectroscopy and magnetic measurements in the temperature interval 5-300 K. Four magnetic quantities viz. hyperfine field, Curie temperature, magnetic moment and susceptibility were determined. The sample containing 34.4 at% V was revealed to exhibit the largest values found up to now for the sigma-phase for average hyperfine field, B = 12.1 T, average magnetic moment per Fe atom, m = 0.89 mB, and Curie temperature, TC = 315.5 K. The quantities were shown to be strongly correlated with each other. In particular, TC is linearly correlated with m with a slope of 406.5 K/mB, as well as B is so correlated with m yielding 14.3 T/mB for the hyperfine coupling constant.
△ Less
Submitted 16 October, 2008;
originally announced October 2008.
-
Anomalous behavior of the Debye temperature in Fe-rich Fe-Cr alloys
Authors:
B. F. O. Costa,
J. Cieslak,
S. M. Dubiel
Abstract:
Debye temperature, $Θ_D$, of Fe-rich Fe$_{100-x}$Cr$_x$ disordered alloys with $0\le x \le 22.3$ was determined from the temperature dependence of the central shift of Mössbauer spectra recorded in the temperature range of 60 -- 300 K. Its compositional dependence shows a maximum at $x \approx 5$ with a relative increase of $\sim 30$% compared to a pure iron. The composition at which the effect…
▽ More
Debye temperature, $Θ_D$, of Fe-rich Fe$_{100-x}$Cr$_x$ disordered alloys with $0\le x \le 22.3$ was determined from the temperature dependence of the central shift of Mössbauer spectra recorded in the temperature range of 60 -- 300 K. Its compositional dependence shows a maximum at $x \approx 5$ with a relative increase of $\sim 30$% compared to a pure iron. The composition at which the effect occurs correlates well with that at which several other quantities, e. g. the Curie temperature and the spin-wave stiffness coefficient, $D_0$, show their maxima, but the enhancement of $Θ_D$ is significantly greater and comparable with the enhancement of the hyperfine field (spin-density of itinerant $s$-like electrons) in the studied system. The results suggest that the electron-phonon interaction is important in this alloy system.
△ Less
Submitted 1 October, 2008;
originally announced October 2008.