Nano-Patterned Pt-Based Metallic Glass Electrocatalysts with In-Situ Copper Oxide Foam for Enhanced Hydrogen Evolution
Authors:
Fei-Fan Cai,
Baran Sarac,
Adnan Akman,
Juan J. Londoño,
Selin Gümrükcü,
Lukas Schweiger,
Martin Hantusch,
Jan Schroers,
Andreas Blatter,
Annett Gebert,
Florian Spieckermann,
Jürgen Eckert
Abstract:
Hydrogen is a promising energy carrier for replacing fossil fuels, and hydrogen production via hydrogen evolution reaction (HER) is an environmentally friendly option if electrocatalysts with low overpotentials and long-term stability are used. In this work, the electrocatalytic performance of $\mathrm{Pt_{57.5}Cu_{14.7}Ni_{5.3}P_{22.5}}$ bulk metallic glass (BMG) with flat, micro-patterned, and n…
▽ More
Hydrogen is a promising energy carrier for replacing fossil fuels, and hydrogen production via hydrogen evolution reaction (HER) is an environmentally friendly option if electrocatalysts with low overpotentials and long-term stability are used. In this work, the electrocatalytic performance of $\mathrm{Pt_{57.5}Cu_{14.7}Ni_{5.3}P_{22.5}}$ bulk metallic glass (BMG) with flat, micro-patterned, and nano-patterned surfaces for HER in 0.5 M H2SO4 is studied. The nano-patterned Pt-BMG demonstrates outstanding long-term stability and self-improving behavior with a final overpotential of 150 mV and a Tafel slope of 42 $\mathrm{mV dec^{-1}}$ after 1000 linear sweep voltammetry (LSV) cycles, which is respectively 42% and 37% lower than in the first LSV cycle. X-ray photoelectron spectroscopy (XPS) and Auger electron spectroscopy (AES) indicate the formation of a layer of CuO/Cu2O foam deposited on top of the nano-patterned surface during the stability test of 1000 LSV cycles. A three-step process is proposed to explain the formation of CuxO foam via dynamic hydrogen bubble templating (DHBT) electrodeposition from Cu dissolution of the Pt-BMG without using copper salt. This work provides a method to create CuxO foams that could be used for various applications. Moreover, nano-patterned BMGs with DHBT deposition offer a feasible strategy to synthesize metal or metal-oxide foams.
△ Less
Submitted 20 June, 2024;
originally announced June 2024.
Corrosion studies on Fe-30Mn-1C alloy in chloridecontaining solutions with view to biomedical application
Authors:
Annett Gebert,
Fabian Kochta,
Andrea Voß,
S. Oswald,
Monica Fernandez-Barcia,
Uta Kühn,
Julia Hufenbach
Abstract:
Austenitic Fe-30Mn-1C (FeMnC) is a prospective biodegradable implant material combining high mechanical integrity with adequate corrosion rates. The fast solidified TWIP alloy, its constituents and 316L stainless steel were electrochemically analysed in various electrolytes at 37 °C under laminar flow. Potentiodynamic polarization tests were conducted in Trisbuffered simulated body fluid (SBF), in…
▽ More
Austenitic Fe-30Mn-1C (FeMnC) is a prospective biodegradable implant material combining high mechanical integrity with adequate corrosion rates. The fast solidified TWIP alloy, its constituents and 316L stainless steel were electrochemically analysed in various electrolytes at 37 °C under laminar flow. Potentiodynamic polarization tests were conducted in Trisbuffered simulated body fluid (SBF), in Tris-buffered saline (TBS) and in 150 mM - 0.15 mM NaCl solutions (pH 7.6, 10, 5, 2) to study initial corrosion stages. Active dissolution of FeMnC is revealed in all electrolytes and is discussed on basis of the Fe and Mn behaviour plus is compared to that of 316L. The role of Tris (Tris(hydroxymethyl)aminomethane) as organic buffer for SBFs is critically assessed, particularly with view to the sensitivity of Fe. SEM studies of FeMnC corroded in NaCl revealed preferential dissolution along Mn-rich grain boundary regions. Static immersion tests of FeMnC in SBF with surface and solution analyses (SEM/EDX, XPS, ICP-OES) indicated that dissolution processes interfere with the formation of permeable surface coatings comprising hydroxides and salts.
△ Less
Submitted 9 April, 2019;
originally announced April 2019.