Cooling Rate Effects on the Structure of 45S5 Bioglass: Computational and Experimental Evidence of Si--P Avoidance
Authors:
Pratik Bhaskar,
Yashasvi Maurya,
Rajesh Kumar,
R. Ravinder,
Amarnath R. Allu,
Sumanta Das,
Nitya Nand Gosvami,
Randall E. Youngman,
Mikkel S. Bødker,
Nerea Mascaraque,
Morten M. Smedskjaer,
Mathieu Bauchy,
N. M. Anoop Krishnan
Abstract:
Due to its ability to bond with living tissues upon dissolution, 45S5 bioglass and related compositions are promising materials for the replacement, regeneration, and repair of hard tissues in the human body. However, the details of their atomic structure remain unclear. This is partially due to the non-equilibrium nature of glasses, as their non-crystalline structure is highly dependent on their…
▽ More
Due to its ability to bond with living tissues upon dissolution, 45S5 bioglass and related compositions are promising materials for the replacement, regeneration, and repair of hard tissues in the human body. However, the details of their atomic structure remain unclear. This is partially due to the non-equilibrium nature of glasses, as their non-crystalline structure is highly dependent on their thermal history, namely, the cooling rate used during quenching. Herein, using molecular dynamics (MD) simulations and magic angle spinning nuclear magnetic resonance (MAS-NMR) spectroscopy experiments, we investigate the structure of the nominal 45S5 bioglass composition prepared using cooling rates ranging over several orders of magnitude. We show that the simulations results are in very good agreement with experimental data, provided that they are extrapolated toward lower cooling rates achieved in experiments. These results highlight that previously reported inconsistencies between simulations and experiments stem from the difference in cooling rate, thereby addressing one of the longstanding questions on the structure of bioglass. Based on these results, we demonstrate the existence of a Si--P avoidance behavior, which may be key in controlling the bioactivity of 45S5 bioglass.
△ Less
Submitted 24 June, 2019;
originally announced June 2019.
Structural Dependence of Chemical Durability in Modified Aluminoborate Glasses
Authors:
Nerea Mascaraque,
Kacper Januchta,
Kristine F. Frederiksen,
Randall E. Youngman,
Mathieu Bauchy,
Morten M. Smedskjaer
Abstract:
Alkali and alkaline earth aluminoborate glasses feature high resistance to cracking under sharp contact loading compared to other oxide glasses. However, due to the high content of hygroscopic B2O3, it is expected that applications of these glasses could be hindered by poor chemical durability in aqueous solutions. Indeed, the compositional and structural dependence of their dissolution kinetics r…
▽ More
Alkali and alkaline earth aluminoborate glasses feature high resistance to cracking under sharp contact loading compared to other oxide glasses. However, due to the high content of hygroscopic B2O3, it is expected that applications of these glasses could be hindered by poor chemical durability in aqueous solutions. Indeed, the compositional and structural dependence of their dissolution kinetics remains unexplored. In this work, we correlate the dissolution rates of aluminoborate glasses in acidic, neutral, and basic solutions with the structural changes induced by varying the aluminum-to-boron ratio. In detail, we investigate a total of seventeen magnesium, lithium, and sodium aluminoborate glasses with fixed modifier content of 25 mol%. We show that the structural changes induced by alumina depend on the network modifier. We also demonstrate a correlation between the chemical durability at various pH values and the structural changes in Mg-, Li- and Na- aluminoborate glasses. The substitution of alumina by boron oxide leads to a general decrease of chemical corrosion in neutral and acidic solutions. The lowest dissolution rate value is observed in Mg-aluminoborate glasses, as a consequence of the intermediate character of magnesium which can increase the network cross-linking. For basic solutions, the chemical durability is almost constant for the different amount of alumina in the three series, likely because B2O3 is susceptible to nucleophilic attack, which is favored in high-OH- solutions.
△ Less
Submitted 14 May, 2018;
originally announced May 2018.