Strengthening of Mg-Al-Ca alloys with C15 and C36 Laves phases
Authors:
Mhammad Zubair,
Stefanie Sandlöbes-Haut,
Risheng Pei,
Maximilian A. Wollenweber,
James S. K-L. Gibson,
S. Korte-Kerzel
Abstract:
The Laves phase skeleton in cast Mg-Al-Ca alloys is known to provide considerable strengthening. Laves phases such as CaMg$_2$ (C14), Ca(Al,Mg)$_2$ (C36), and CaAl2 (C15) have high melting points, high hardness at room and elevated temperatures, but unfortunately are inherently brittle. Mg-Al-Ca alloys thus have good creep properties but limited ductility. An understanding of the co-deformation be…
▽ More
The Laves phase skeleton in cast Mg-Al-Ca alloys is known to provide considerable strengthening. Laves phases such as CaMg$_2$ (C14), Ca(Al,Mg)$_2$ (C36), and CaAl2 (C15) have high melting points, high hardness at room and elevated temperatures, but unfortunately are inherently brittle. Mg-Al-Ca alloys thus have good creep properties but limited ductility. An understanding of the co-deformation behaviour of $α$-Mg and Laves phases is essential for optimising the strength-ductility balance of these alloys. Here, we study the mechanical behaviour of a Mg-4.65Al-2.82Ca alloy using micropillar compression in the $α$-Mg matrix, at $α$-Mg/C36 and $α$-Mg/C15 interfaces and in the C15 phase in combination with scanning electron microscopy (SE imaging), electron backscatter diffraction (EBSD), transmission Kikuchi diffraction (TKD), and low-kV scanning transmission electron microscopy (STEM). We show that both, C15 and C36, Laves phases provide considerable strengthening to the $α$-Mg matrix by delaying the onset of basal slip and extension twinning, while only the C36 phase appears to allow a certain extent of slip transfer/ plastic co-deformation, in spite of its greater anisotropy compared with the cubic C15 phase. We therefore conclude based on these results that strengthening of the $α$-Mg matrix by the C36 Laves phase is preferable given that it combines easy skeleton formation with some co-deformation and considerable stability at common application temperatures of magnesium alloys.
△ Less
Submitted 9 February, 2023;
originally announced February 2023.
-
Co-deformation Between the Metallic Matrix and Intermetallic Phases in a Creep-Resistant Mg-3.68Al-3.8Ca Alloy
Authors:
M. Zubair,
S. Sandlöbes-Haut,
M. Lipińska-Chwałek,
M. A. Wollenweber,
C. Zehnder,
J. Mayer,
J. S. K-L. Gibson,
S. Korte-Kerzel
Abstract:
The microstructure of Mg-Al-Ca alloys consists of a hard intra- and intergranular eutectic Laves phase network embedded in a soft $α$-Mg matrix. For such heterogeneous microstructures, the mechanical response and co-deformation of both phases under external load are not yet fully understood. We therefore used nano- and microindentation in combination with electron microscopy to study the deformati…
▽ More
The microstructure of Mg-Al-Ca alloys consists of a hard intra- and intergranular eutectic Laves phase network embedded in a soft $α$-Mg matrix. For such heterogeneous microstructures, the mechanical response and co-deformation of both phases under external load are not yet fully understood. We therefore used nano- and microindentation in combination with electron microscopy to study the deformation behaviour of an Mg-3.68Al-3.8Ca alloy.
We found that the hardness of the Mg$_2$Ca phase was significantly larger than the $α$-Mg phase and stays constant within the measured temperature range. The strain rate sensitivity of the softer $α$-Mg phase and of the interfaces increased while activation volume decreased with temperature. The creep deformation of the Mg$_2$Ca Laves phase was significantly lower than the $α$-Mg phase at 170 $^{\circ}$C. Moreover, the deformation zone around and below microindents depends on the matrix orientation and is influenced by the presence of Laves phases. Most importantly, slip transfer from the $α$-Mg phase to the (Mg,Al)$_2$Ca Laves phase occurred, carried by the basal planes. Based on the observed orientation relationship and active slip systems, a slip transfer mechanism from the soft $α$-Mg phase to the hard Laves phase is proposed. Further, we present implications for future alloy design strategies.
△ Less
Submitted 30 August, 2021;
originally announced August 2021.
-
Strain heterogeneity and micro-damage nucleation under tensile stresses in an Mg-5Al-3Ca alloy with an intermetallic skeleton
Authors:
Muhammad Zubair,
Stefanie Sandlöbes-Haut,
Max A. Wollenweber,
Katrin Bugelnig,
Carl F. Kusche,
Guillermo Requena,
Sandra Korte-Kerzel
Abstract:
Strain heterogeneity at the microstructural level plays a vital role in the deformation and fracture behaviour of dual or multi-phase materials. In the present work, the strain heterogeneity, localization and partitioning arising at the sub-micron scale during elevated temperature (170 °C) tensile deformation of an Mg-5Al-3Ca alloy was investigated using quasi in-situ μ-DIC experiments. The result…
▽ More
Strain heterogeneity at the microstructural level plays a vital role in the deformation and fracture behaviour of dual or multi-phase materials. In the present work, the strain heterogeneity, localization and partitioning arising at the sub-micron scale during elevated temperature (170 °C) tensile deformation of an Mg-5Al-3Ca alloy was investigated using quasi in-situ μ-DIC experiments. The results reveal that the strain is mainly carried by the α-Mg phase, while the intermetallic Laves phase plays a critical role in that strain concentrations build up at the α-Mg matrix and Laves phase interfaces, hence, reducing the overall deformability of the alloy. In quasi in-situ and bulk material analysis at elevated temperature, cracks were observed to nucleate in the Laves phase, at i) the intersection points of slip lines in the α-Mg matrix with the Laves phase and ii) the twin intersections with α-Mg/Laves phase interfaces and iii) twin transmissions across α-Mg/Laves phase interfaces. Euler number analysis has shown that the (inter-)connectivity of the Laves phase decreases with deformation. Finally, cracks grow preferentially along the Laves phases until the material fractures.
△ Less
Submitted 22 August, 2019;
originally announced August 2019.