Prediction and identification of point defect fingerprints in the X-ray photoelectron spectra of TiN$_x$
Authors:
Pavel Ondračka,
Pauline Kümmerl,
Marcus Hans,
Stanislav Mráz,
Daniel Primetzhofer,
David Holec,
Petr Vašina,
Jochen M. Schneider
Abstract:
We investigate the effect of selected N and Ti point defects in $B$1 TiN on N 1s and Ti 2p$_{3/2}$ binding energies (BE) by experiments and ab initio calculations. X-ray photoelectron spectroscopy (XPS) measurements of Ti-deficient TiN films reveal additional N 1s spectral components at lower binding energies. Ab initio calculations predict that these components are caused by either Ti vacancies,…
▽ More
We investigate the effect of selected N and Ti point defects in $B$1 TiN on N 1s and Ti 2p$_{3/2}$ binding energies (BE) by experiments and ab initio calculations. X-ray photoelectron spectroscopy (XPS) measurements of Ti-deficient TiN films reveal additional N 1s spectral components at lower binding energies. Ab initio calculations predict that these components are caused by either Ti vacancies, which induce a N 1s BE shift of $-0.53$ eV in its first N neighbors, and/or N tetrahedral interstitials, which have their N 1s BE shifted by $-1.18$ eV and also shift BE of their first N neighbors by $-0.53$ eV. However, the {\it ab initio} calculations also reveal that the tetrahedral N interstitial is unstable at room temperature. We, therefore, unambiguously attribute the detected signal to Ti vacancies. Furthermore, the vacancy concentration in Ti-deficient TiN was quantified with XPS supported by ab initio calculations. The largest BE shifts of $-1.53$, $-1.80$ and $-2.28$ eV for Ti 2p$_{3/2}$ electrons are predicted for the Ti tetrahedral, split (10$\overline{1}$)-aligned and split (111)-aligned interstitial atoms, respectively, and we, therefore, propose XPS could detect them. Other defects such as N vacancy or N split (10$\overline{1}$)-aligned interstitial introduce smaller N 1s and Ti 2p$_{3/2}$ BE shifts and are unlikely to be detectable experimentally. Our work highlights the potential of ab initio-guided XPS measurements in detecting and quantifying point defects in $B$1 TiN.
△ Less
Submitted 28 March, 2024;
originally announced March 2024.
-
Large-area deposition of protective (Ti,Al)N coatings onto polycarbonate
Authors:
Lena Patterer,
Sabrina Kollmann,
Teresa de los Arcos,
Leonie Jende,
Soheil Karimi Aghda,
Damian M. Holzapfel,
Sameer Aman Salman,
Stanislav Mráz,
Guido Grundmeier,
Jochen M. Schneider
Abstract:
Polycarbonate (PC) and protective (Ti,Al)N coatings exhibit extremely different material properties, specifically crystal structure, thermal stability, elastic and plastic behavior as well as thermal expansion coefficients. These differences present formidable challenges for the deposition process development as low-temperature synthesis routes have to be explored to avoid a thermal overload of th…
▽ More
Polycarbonate (PC) and protective (Ti,Al)N coatings exhibit extremely different material properties, specifically crystal structure, thermal stability, elastic and plastic behavior as well as thermal expansion coefficients. These differences present formidable challenges for the deposition process development as low-temperature synthesis routes have to be explored to avoid a thermal overload of the polymer substrate. Here, a large-area sputtering process is developed to address the challenges by systematically adjusting target peak power density and duty cycle. Adhering (Ti,Al)N coatings with a critical residual tensile stress of 2.2 +/- 0.2 GPa are obtained in the pulsed direct current magnetron sputtering range, whereas depositions at higher target peak power densities, realized by high power pulsed magnetron sputtering, lead to stress-induced adhesive and/or cohesive failure. The stress-optimized (Ti,Al)N coatings deposited onto PC with a target peak power density of 0.036 kW cm-2 and a duty cycle of 5.3% were investigated by cross-cut test confirming adhesion. By investigating the bond formation at the PC | (Ti,Al)N interface, mostly interfacial CNx bonds and a small fraction of (C-O)-(Ti,Al) bonds are identified by X-ray photoelectron spectroscopy, indicating reactions at the hydrocarbon and the carbonate groups during deposition. Nanoindentation reveals an elastic modulus of 296 +/- 18 GPa for the (Ti,Al)N coating, while a Ti-Al-O layer is formed during electrochemical impedance spectroscopy in a borate buffer solution, indicating protective passivation. This work demonstrates that the challenge posed by the extremely different material properties at the interface of soft polymer substrates and hard coatings can be addressed by systematical variation of the pulsing parameters to reduce the residual film stress.
△ Less
Submitted 27 May, 2023;
originally announced May 2023.
-
Bond formation at polycarbonate | X interfaces (X = Al$_2$O$_3$, TiO$_2$, TiAlO$_2$) studied by theory and experiments
Authors:
Lena Patterer,
Pavel Ondračka,
Dimitri Bogdanovski,
Stanislav Mráz,
Peter J. Pöllmann,
Soheil Karimi Aghda,
Petr Vašina,
Jochen M. Schneider
Abstract:
Interfacial bond formation during sputter deposition of metal oxide thin films onto polycarbonate (PC) is investigated by ab initio molecular dynamics simulations and X-ray photoelectron spectroscopy (XPS) analysis of PC | X interfaces (X = Al$_2$O$_3$, TiO$_2$, TiAlO$_2$). Generally, the predicted bond formation is consistent with the experimental data. For all three interfaces, the majority of b…
▽ More
Interfacial bond formation during sputter deposition of metal oxide thin films onto polycarbonate (PC) is investigated by ab initio molecular dynamics simulations and X-ray photoelectron spectroscopy (XPS) analysis of PC | X interfaces (X = Al$_2$O$_3$, TiO$_2$, TiAlO$_2$). Generally, the predicted bond formation is consistent with the experimental data. For all three interfaces, the majority of bonds identified by XPS are (C-O)-metal bonds, whereas C-metal bonds are the minority. Compared to the PC | Al$_2$O$_3$ interface, the PC | TiO$_2$ and PC | TiAlO$_2$ interfaces exhibit a reduction in the measured interfacial bond density by ~ 75 and ~ 65%, respectively. Multiplying the predicted bond strength with the corresponding experimentally determined interfacial bond density shows that Al$_2$O$_3$ exhibits the strongest interface with PC, while TiO$_2$ and TiAlO$_2$ exhibit ~ 70 and ~ 60% weaker interfaces, respectively. This can be understood by considering the complex interplay between the metal oxide composition, the bond strength as well as the population of bonds that are formed across the interface.
△ Less
Submitted 27 May, 2023;
originally announced May 2023.
-
Correlative Theoretical and Experimental Study of the Polycarbonate | X Interfacial Bond Formation (X = AlN, TiN, TiAlN) during Magnetron Sputtering
Authors:
Lena Patterer,
Pavel Ondračka,
Dimitri Bogdanovski,
Stanislav Mráz,
Soheil Karimi Aghda,
Peter J. Pöllmann,
Yu-** Chien,
Jochen M. Schneider
Abstract:
To understand the interfacial bond formation between polycarbonate (PC) and magnetron-sputtered metal nitride thin films, PC | X interfaces (X = AlN, TiN, TiAlN) are comparatively investigated by ab initio simulations as well as X-ray photoelectron spectroscopy. The simulations predict significant differences at the interface, as N and Ti form bonds with all functional groups of the polymer, while…
▽ More
To understand the interfacial bond formation between polycarbonate (PC) and magnetron-sputtered metal nitride thin films, PC | X interfaces (X = AlN, TiN, TiAlN) are comparatively investigated by ab initio simulations as well as X-ray photoelectron spectroscopy. The simulations predict significant differences at the interface, as N and Ti form bonds with all functional groups of the polymer, while Al reacts selectively only with the carbonate group of pristine PC. In good agreement with simulations, experimental data reveal that the PC | AlN and the PC | TiAlN interfaces are mainly defined by interfacial C-N bonds, whereas for PC | TiN, the interface formation is also characterized by numerous C-Ti and (C-O)-Ti bonds. Bond strength calculations combined with the measured interfacial bond density indicate the strongest interface for PC | TiAlN followed by PC | AlN, whereas the weakest is predicted for PC | TiN due to its lower density of strong interfacial C-N bonds. This study shows that the employed computational strategy enables prediction of the interfacial bond formation between PC and metal nitrides and that it is reasonable to assume that the research strategy proposed herein can be readily adapted to other organic | inorganic interfaces.
△ Less
Submitted 26 May, 2023;
originally announced May 2023.
-
Early stages of dissolution corrosion in 316L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500$^\circ$C
Authors:
Evangelia Charalampopoulou,
Konstantina Lambrinou,
Tom Van der Donck,
Boris Paladino,
Fabio Di Fonzo,
Clio Azina,
Per Eklund,
Stanislav Mráz,
Jochen M. Schneider,
Dominique Schryvers,
Rémi Delville
Abstract:
This work addresses the early stages ($\le$1000 h) of the dissolution corrosion behavior of 316L and DIN 1.4970 austenitic stainless steels in contact with oxygen-poor (C$_O$ < 10$^-$$^8$ mass%), static liquid lead-bismuth eutectic (LBE) at 500°C for 600-1000 h. The objective of this study was to determine the relative early-stage resistance of the uncoated steels to dissolution corrosion and to a…
▽ More
This work addresses the early stages ($\le$1000 h) of the dissolution corrosion behavior of 316L and DIN 1.4970 austenitic stainless steels in contact with oxygen-poor (C$_O$ < 10$^-$$^8$ mass%), static liquid lead-bismuth eutectic (LBE) at 500°C for 600-1000 h. The objective of this study was to determine the relative early-stage resistance of the uncoated steels to dissolution corrosion and to assess the protectiveness of select candidate coatings (Cr$_2$AlC, Al$_2$O$_3$, V$_2$Al$_x$C$_y$). The simultaneous exposure of steels with intended differences in microstructure and thermomechanical state showed the effects of steel grain size, density of annealing/deformation twins, and secondary precipitates on the steel dissolution corrosion behavior. The findings of this study provide recommendations on steel manufacturing with the aim of using the steels to construct Gen-IV lead-cooled fast reactors.
△ Less
Submitted 13 July, 2021;
originally announced August 2021.