Permanent Magnets Based on Hard Ferrite Ceramics
Authors:
Cecilia Granados-Miralles,
Matilde Saura-Múzquiz,
Henrik L. Andersen
Abstract:
Permanent magnets are integral components in many of the modern technologies that are critical for the transition to a sustainable society. However, most of the high-performance (BHmax > 100 kJ/m3) permanent magnets that are currently employed contain rare earth elements (REE), which have long been classified as critical materials with a high supply risk and concerns regarding pollution in their m…
▽ More
Permanent magnets are integral components in many of the modern technologies that are critical for the transition to a sustainable society. However, most of the high-performance (BHmax > 100 kJ/m3) permanent magnets that are currently employed contain rare earth elements (REE), which have long been classified as critical materials with a high supply risk and concerns regarding pollution in their mining. Therefore, suitable REE-lean/free magnets must be developed in order to ensure the sustainability of clean energy generation and electric mobility. The REE-free hexagonal ferrites (or hexaferrites) are the most used permanent magnets across all applications, with an 85 wt.% pie of the permanent magnet market. They are the dominant lower-grade option (BHmax < 25 kJ/m3) due to their relatively good hard magnetic properties, high Curie temperature (>700 K), low cost and good chemical stability. In recent years, the hexaferrites have also emerged as candidates for substituting REE-based permanent magnets in applications requiring intermediate magnetic performance (25-100 kJ/m3), due to considerable performance improvements achieved through chemical tuning, nanostructuring and compaction/sintering optimization. This chapter reviews the state-of-the-art sintering strategies being investigated with the aim of manufacturing hexaferrite magnets with optimized magnetic properties, identifying key challenges and highlighting the natural future steps to be followed.
△ Less
Submitted 3 October, 2023;
originally announced October 2023.
-
Dense strontium hexaferrite-based permanent magnet composites assisted by cold sintering process
Authors:
Eduardo García-Martín,
Cecilia Granados-Miralles,
Sandra Ruiz-Gómez,
Lucas Pérez,
Adolfo del Campo,
Jesús Carlos Guzmán-Mínguez,
César de Julián Fernández,
Adrián Quesada,
José F. Fernández,
Aida Serrano
Abstract:
The use of rare-earth-based permanent magnets is one of the critical points for the development of the current technology. On the one hand, industry of the rare-earths is highly polluting due to the negative environmental impact of their extraction and, on the other hand, the sector is potentially dependent on China. Therefore, investigation is required both in the development of rare-earth-free p…
▽ More
The use of rare-earth-based permanent magnets is one of the critical points for the development of the current technology. On the one hand, industry of the rare-earths is highly polluting due to the negative environmental impact of their extraction and, on the other hand, the sector is potentially dependent on China. Therefore, investigation is required both in the development of rare-earth-free permanent magnets and in sintering processes that enable their greener fabrication with attractive magnetic properties at a more competitive price. This work presents the use of a cold sintering process (CSP) followed by a post-annealing at 1100 °C as a new way to sinter composite permanent magnets based on strontium ferrite (SFO). Composites that incorporate a percentage < 10% of an additional magnetic phase have been prepared and the morphological, structural and magnetic properties have been evaluated after each stage of the process. CSP induces a phase transformation of SFO in the composites, which is partially recovered by the post-thermal treatment improving the relative density to 92% and the magnetic response of the final magnets with a coercivity of up to 3.0 kOe. Control of the magnetic properties is possible through the composition and the grain size in the sintered magnets. These attractive results show the potential of the sintering approach as an alternative to develop modern rare-earth-free composite permanent magnets.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
In-depth investigations of size and occupancies in cobalt ferrite nanoparticles by joint Rietveld refinements of X-ray and neutron powder diffraction data
Authors:
K. Henry,
J. V. Ahlburg,
H. L. Andersen,
C. Granados-Miralles,
M. Stingaciu,
M. Saura-Múzquiz,
M. Christensen
Abstract:
Powder X-ray diffraction (PXRD) and neutron powder diffraction (NPD) have been used to investigate the crystal structure of CoFe2O4 nanoparticles prepared via different hydrothermal synthesis routes, with particular attention given to accurately determining the spinel inversion degrees. The study is divided into four parts. In the first part, the investigations focus on the influence of using diff…
▽ More
Powder X-ray diffraction (PXRD) and neutron powder diffraction (NPD) have been used to investigate the crystal structure of CoFe2O4 nanoparticles prepared via different hydrothermal synthesis routes, with particular attention given to accurately determining the spinel inversion degrees. The study is divided into four parts. In the first part, the investigations focus on the influence of using different diffraction pattern combinations (NPD, Cu-source PXRD and Co-source PXRD) for the structural modelling. It is found that combining PXRD data from a Co source with NPD data offers a robust structural model. The second part of the study evaluates the reproducibility of the employed multipattern Rietveld refinement procedure using different data sets collected on the same sample, as well as on equivalently prepared samples. The refinement procedure gives reproducible results and reveals that the synthesis method is likewise reproducible since only minor differences are noted between the samples. The third part focuses on the structural consequences of (i) the employed heating rate (achieved using three different hydrothermal reactor types) and (ii) changing the cobalt salt in the precursors [aqueous salt solutions of Co(CH3COOH)2, Co(NO3)2 and CoCl2] in the synthesis. It is found that increasing the heating rate causes a change in the crystal structure (unit cell and crystallite sizes) while the Co/Fe occupancy and magnetic parameters remain similar in all cases. Also, changing the type of cobalt salt does not alter the final crystal/magnetic structure of the CoFe2O4 nanoparticles. The last part of this study is a consideration of the chemicals and parameters used in the synthesis of the different samples.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Greener processing of SrFe$_{12}$O$_{19}$ ceramic permanent magnets by two-step sintering
Authors:
J. C. Guzmán-Mínguez,
V. Fuertes,
C. Granados-Miralles,
J. F. Fernández,
A. Quesada
Abstract:
With an annual production amounting to 800 kilotons, ferrite magnets constitute the largest family of permanent magnets in volume, a demand that will only increase as a consequence of the rare-earth crisis. With the global goal of building a climate-resilient future, strategies towards a greener manufacturing of ferrite magnets are of great interest. A new ceramic processing route for obtaining de…
▽ More
With an annual production amounting to 800 kilotons, ferrite magnets constitute the largest family of permanent magnets in volume, a demand that will only increase as a consequence of the rare-earth crisis. With the global goal of building a climate-resilient future, strategies towards a greener manufacturing of ferrite magnets are of great interest. A new ceramic processing route for obtaining dense Sr-ferrite sintered magnets is presented here. Instead of the usual sintering process employed nowadays in ferrite magnet manufacturing that demands long dwell times, a shorter two-step sintering is designed to densify the ferrite ceramics. As a result of these processes, dense SrFe$_{12}$O$_{19}$ ceramic magnets with properties comparable to state-of-the-art ferrite magnets are obtained. In particular, the SrFe$_{12}$O$_{19}$ magnet containing 0.2% PVA and 0.6% wt SiO$_2$ reaches a coercivity of 164 kA/m along with a 93% relative density. A reduction of 31% in energy consumption is achieved in the thermal treatment with respect to conventional sintering, which could lead to energy savings for the industry of the order of 7.109 kWh per year.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Effect of organic solvent on the cold sintering processing of SrFe12O19 platelet-based permanent magnets
Authors:
Aida Serrano,
Eduardo García-Martín,
Cecilia Granados-Miralles,
Jesús López-Sánchez,
Giulio Gorni,
Adrián Quesada,
José F. Fernández
Abstract:
In this work we have investigated the effect of the solvent during the processing of SrFe12O19 platelet-based permanent magnets by cold sintering process (CSP) plus a post-thermal treatment. Several organic solvents: glacial acetic acid, oleic acid and oleylamine have been analyzed, optimizing the CSP temperatures at 190-270 °C, under pressures of 375-670 MPa and 6-50 wt% of solvent. Modifications…
▽ More
In this work we have investigated the effect of the solvent during the processing of SrFe12O19 platelet-based permanent magnets by cold sintering process (CSP) plus a post-thermal treatment. Several organic solvents: glacial acetic acid, oleic acid and oleylamine have been analyzed, optimizing the CSP temperatures at 190-270 °C, under pressures of 375-670 MPa and 6-50 wt% of solvent. Modifications in the morphological and structural properties are identified depending on the solvent, which impacts on the magnetic response. Independently of the solvent, the mechanical integrity of ferrite magnets obtained by CSP is improved by a post-annealing at 1100 °C for 2 h, resulting in relative densities around 92 % with an average grain size of 1 μm and a fraction of SrFe12O19 phase > 91 %. Hc > 2.1 kOe and MS of 73 emu/g are obtained in the final sintered ceramic magnets, exhibiting the highest HC value of 2.8 kOe for the magnet sintered using glacial acetic acid.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Novel one-pot sol-gel synthesis route of Fe3C/few-layered graphene core/shell nanoparticles embedded in a carbon matrix
Authors:
Alberto Castellano-Soria,
Jesús López-Sánchez,
Cecilia Granados-Miralles,
María Varela,
Elena Navarro,
César González,
Pilar Marín
Abstract:
Fe3C/few-layered graphene core/shell nanoparticles embedded in a carbon matrix are synthesized by a novel two-step surfactant sol-gel strategy, where the processes of hydrolysis, polycondensation and drying take place in a one-pot. The present approach is based on the combined action of oleic acid and oleylamine, which act sterically on the precursor micelles when a densification temperature is pe…
▽ More
Fe3C/few-layered graphene core/shell nanoparticles embedded in a carbon matrix are synthesized by a novel two-step surfactant sol-gel strategy, where the processes of hydrolysis, polycondensation and drying take place in a one-pot. The present approach is based on the combined action of oleic acid and oleylamine, which act sterically on the precursor micelles when a densification temperature is performed in a reducing atmosphere. The structural and magnetic evolution of the formed compounds is investigated, ranging from iron oxides such as Fe3O4 and FeO, to the formation of pure Fe3C/C samples from 700 °C onwards. Interestingly, Fe3C nanoparticles with a size of ~20 nm crystallize immersed in the carbon matrix and the surrounding environment forms an oriented encapsulation built by few-layered graphene. The nanostructures show a saturation magnetization of ~43 emu/g and a moderate coercivity of ~500 Oe. Thereby, an innovative chemical route to produce single phase Fe3C nanoparticles is described, and an effective method of few-layered graphene passivation is proposed, yielding a product with a high magnetic response and high chemical stability against environmental corrosion.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
On the potential of hard ferrite ceramics for permanent magnet technology -- a review on sintering strategies
Authors:
Cecilia Granados-Miralles,
Petra Jenuš
Abstract:
A plethora of modern technologies rely on permanent magnets for their operation, including many related to the transition towards a sustainable future, such as wind turbines or electric vehicles. Despite the overwhelming superiority of magnets based on rare-earth elements in terms of the magnetic performance, the harmful environmental impact of the mining of these raw materials, their uneven distr…
▽ More
A plethora of modern technologies rely on permanent magnets for their operation, including many related to the transition towards a sustainable future, such as wind turbines or electric vehicles. Despite the overwhelming superiority of magnets based on rare-earth elements in terms of the magnetic performance, the harmful environmental impact of the mining of these raw materials, their uneven distribution on Earth and various political conflicts among countries leave no option but seeking for rare-earth-free alternatives. The family of the hexagonal ferrites or hexaferrites, and in particular the barium and strontium M-type ferrites (BaFe12O19 and SrFe12O19), are strong candidates for a partial rare-earth magnets substitution, and they are indeed successfully implemented in multiple applications. The manufacturing of hexaferrites into dense pieces (i.e. magnets) meeting the requirements of the specific application (e.g. magnetic and mechanical properties, shape) is not always straightforward, which has in many cases hampered the actual substitution at the industrial level. Here, past and on-going research on hexaferrites sintering is reviewed with a historical perspective, focusing on the challenges encountered and the solutions explored, and correlating the sintering approaches with the magnetic performance of the resulting ceramic magnet.
△ Less
Submitted 27 September, 2023;
originally announced September 2023.
-
CoSb3-based skutterudite nanocomposites prepared by cold sintering process with enhanced thermoelectric properties
Authors:
Aida Serrano,
Olga Caballero-Calero,
Cecilia Granados-Miralles,
Giulio Gorni,
Cristina V. Manzano,
Marta Rull-Bravo,
Alberto Moure,
Marisol Martín-González,
José F. Fernández
Abstract:
We show here for the first time the use of a cold sintering process (CSP) to sinter CoSb3-based thermoelectric materials. CSP at 150 °C for 90 min under a uniaxial pressure of 750 MPa yields pieces with a relative density of 86 %, which is increased to around 92 % after a post-annealing at temperatures > 500 °C in Ar atmosphere. The reported CSP produces Te doped-CoSb3 nanocomposites with similar…
▽ More
We show here for the first time the use of a cold sintering process (CSP) to sinter CoSb3-based thermoelectric materials. CSP at 150 °C for 90 min under a uniaxial pressure of 750 MPa yields pieces with a relative density of 86 %, which is increased to around 92 % after a post-annealing at temperatures > 500 °C in Ar atmosphere. The reported CSP produces Te doped-CoSb3 nanocomposites with similar morphological and structural characteristics to the starting nanopowders obtained by ball milling in air atmosphere. The post-thermal treatment induces grain coalescence and grain growth, crystallite size growth as well as compositional changes in the nanocomposite, decreasing the amount of the main phase, CoSb3, and increasing the weight of secondary phase, CoSb2, up to a 30 wt% at 600 °C. Remarkably, the average valence for the Co, Sb and Te absorbing atoms is neither transformed by the sintering process nor by the subsequent heat treatment. The functional response of the sintered thermoelectric nanocomposites exhibits a maximum figure of merit of 0.12(3) at room temperature for the nanocomposites sintered by CSP with a subsequent post-annealing at 500 °C. This is mainly due to its low thermal conductivity in comparison with similar powders sintered by other approaches, and it is explained by the morphological and structural properties. These findings represent an attractive alternative for obtaining efficient thermoelectric skutterudites by a scalable and cost-effective route.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Quantifying Li-content for compositional tailoring of lithium ferrite ceramics
Authors:
C. Granados-Miralles,
A. Serrano,
P. Prieto,
J. Guzmán-Mínguez,
J. E. Prieto,
A. M. Friedel,
E. García-Martín,
J. F. Fernández,
A. Quesada
Abstract:
Owing to their multiple applications, lithium ferrites are relevant materials for several emerging technologies. For instance, LiFeO2 has been spotted as an alternative cathode material in Li-ion batteries, while LiFe5O8 is the lowest dam** ferrite, holding promise in the field of spintronics. The Li-content in lithium ferrites has been shown to greatly affect the physical properties, and in tur…
▽ More
Owing to their multiple applications, lithium ferrites are relevant materials for several emerging technologies. For instance, LiFeO2 has been spotted as an alternative cathode material in Li-ion batteries, while LiFe5O8 is the lowest dam** ferrite, holding promise in the field of spintronics. The Li-content in lithium ferrites has been shown to greatly affect the physical properties, and in turn, the performance of functional devices based on these materials. Despite this, lithium content is rarely accurately quantified, as a result of the low number of electrons in Li hindering its identification by means of routine materials characterization methods. In the present work, magnetic lithium ferrite powders with Li:Fe ratios of 1:1, 1:3 and 1:5 have been synthesized, successfully obtaining phase-pure materials (LiFeO2 and LiFe5O8), as well as a controlled mixture of both phases. The powders have been compacted and subsequently sintered by thermal treatment (Tmax = 1100 °C) to fabricate dense pellets which preserve the original Li:Fe ratios. Li-content on both powders and pellets has been determined by two independent methods: (i) Rutherford backscattering spectroscopy combined with nuclear reaction analysis and (ii) Rietveld analysis of powder X-ray diffraction data. With good agreement between both techniques, it has been confirmed that the Li:Fe ratios employed in the synthesis are maintained in the sintered ceramics. The same conclusion is drawn from spatially-resolved confocal Raman microscopy experiments on regions of a few microns. Field emission scanning electron microscopy has evidenced the substantial grain growth taking place during the sintering process - mean particle sizes rise from about 600 nm in the powders up to 3.8(6) um for dense LiFeO2 and 10(2) um for LiFe5O8 ceramics.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
A Platform for Addressing Individual Magnetite Islands Grown Epitaxially on Ru(0001) and Manipulating Their Magnetic Domains
Authors:
Sandra Ruiz-Gómez,
Eva María Trapero,
Claudia Fernández-González,
Adolfo del Campo,
Cecilia Granados-Miralles,
José Emilio Prieto,
Muhammad Waqas Khaliq,
Miguel Angel Niño,
Michael Foerster,
Lucía Aballe,
Juan de la Figuera
Abstract:
We have grown high-quality magnetite micrometric islands on ruthenium stripes on sapphire through a combination of magnetron sputtering (Ru film), high-temperature molecular beam epitaxy (oxide islands), and optical lithography. The samples have been characterized by atomic force microscopy, Raman spectroscopy, X-ray absorption and magnetic circular dichroism in a photoemission microscope. The mag…
▽ More
We have grown high-quality magnetite micrometric islands on ruthenium stripes on sapphire through a combination of magnetron sputtering (Ru film), high-temperature molecular beam epitaxy (oxide islands), and optical lithography. The samples have been characterized by atomic force microscopy, Raman spectroscopy, X-ray absorption and magnetic circular dichroism in a photoemission microscope. The magnetic domains on the magnetite islands can be modified by the application of current pulses through the Ru stripes in combination with magnetic fields. The modification of the magnetic domains is explained by the Oersted field generated by the electrical current flowing through the stripes underneath the magnetite nanostructures. The fabrication method is applicable to a wide variety of rock salt and spinel oxides.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Approaching Ferrite-Based Exchange-Coupled Nanocomposites as Permanent Magnets
Authors:
Cecilia Granados-Miralles,
Matilde Saura-Múzquiz,
Henrik L. Andersen,
Adrián Quesada,
Jakob V. Ahlburg,
Ann-Christin Dippel,
Emmanuel Canévet,
Mogens Christensen
Abstract:
During the past decade, CoFe2O4 (hard)/Co-Fe alloy (soft) magnetic nanocomposites have been routinely prepared by partial reduction of CoFe2O4 nanoparticles. Monoxide (i.e., FeO or CoO) has often been detected as a byproduct of the reduction, although it remains unclear whether the formation of this phase occurs during the reduction itself or at a later stage. Here, a novel reaction cell was desig…
▽ More
During the past decade, CoFe2O4 (hard)/Co-Fe alloy (soft) magnetic nanocomposites have been routinely prepared by partial reduction of CoFe2O4 nanoparticles. Monoxide (i.e., FeO or CoO) has often been detected as a byproduct of the reduction, although it remains unclear whether the formation of this phase occurs during the reduction itself or at a later stage. Here, a novel reaction cell was designed to monitor the reduction in situ using synchrotron powder X-ray diffraction (PXRD). Sequential Rietveld refinements of the in situ data yielded time-resolved information on the sample composition and confirmed that the monoxide is generated as an intermediate phase. The macroscopic magnetic properties of samples at different reduction stages were measured by means of vibrating sample magnetometry (VSM), revealing a magnetic softening with increasing soft phase content, which was too pronounced to be exclusively explained by the introduction of soft material in the system. The elemental compositions of the constituent phases were obtained from joint Rietveld refinements of ex situ high-resolution PXRD and neutron powder diffraction (NPD) data. It was found that the alloy has a tendency to emerge in a Co-rich form, inducing a Co deficiency on the remaining spinel phase, which can explain the early softening of the magnetic material.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Expanding the tunability and applicability of exchange-coupled/decoupled magnetic nanocomposites
Authors:
Cecilia Granados-Miralles,
Adrián Quesada,
Matilde Saura-Múzquiz,
Henrik L. Andersen,
José F. Fernández,
Mogens Christensen
Abstract:
CoFe2O4/Co-Fe magnetic composites are usually prepared through partial reduction of CoFe2O4, which often yields monoxides (i.e., FeO, CoO) as secondary phases. Since these compounds are paramagnetic at ambient conditions, the presence of a small amount of monoxide is generally downplayed in the literature, and the possible effects on the magnetic properties are simply ignored. However, the present…
▽ More
CoFe2O4/Co-Fe magnetic composites are usually prepared through partial reduction of CoFe2O4, which often yields monoxides (i.e., FeO, CoO) as secondary phases. Since these compounds are paramagnetic at ambient conditions, the presence of a small amount of monoxide is generally downplayed in the literature, and the possible effects on the magnetic properties are simply ignored. However, the present study shows that even a low concentration of monoxide results in decoupling of the soft and hard magnetic phases, which inevitably leads to a deterioration of the magnetic properties. Additionally, it is confirmed that a partial reduction of CoFe2O4 is a suitable method to produce CoFe2O4/Co-Fe nanocomposites, provided that the treatment is well controlled with respect to duration, temperature and flow of reductant. A monoxide-free nanocomposite was produced and its magnetic properties evaluated both at room and low temperature. Our model system exemplifies the potential of exchange-coupling (and decoupling) as a tool to tune the magnetic properties of a material within a relatively wide range of values, thus widening its spectrum of potential applications.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
FeCo Nanowire-Strontium Ferrite Powder Composites for Permanent Magnets with High-Energy Products
Authors:
J. C. Guzmán-Mínguez,
S. Ruiz-Gómez,
L. M. Vicente-Arche,
C. Granados-Miralles,
C. Fernández-González,
F. Mompeán,
M. García-Hernández,
S. Erohkin,
D. Berkov,
D. Mishra,
C. de Julián Fernández,
J. F. Fernández,
L. Pérez,
A. Quesada
Abstract:
Due to the issues associated with rare-earth elements, there arises a strong need for magnets with properties between those of ferrites and rare-earth magnets that could substitute the latter in selected applications. Here, we produce a high remanent magnetization composite bonded magnet by mixing FeCo nanowire powders with hexaferrite particles. In the first step, metallic nanowires with diameter…
▽ More
Due to the issues associated with rare-earth elements, there arises a strong need for magnets with properties between those of ferrites and rare-earth magnets that could substitute the latter in selected applications. Here, we produce a high remanent magnetization composite bonded magnet by mixing FeCo nanowire powders with hexaferrite particles. In the first step, metallic nanowires with diameters between 30 and 100 nm and length of at least 2 μm are fabricated by electrodeposition. The oriented as-synthesized nanowires show remanence ratios above 0.76 and coercivities above 199 kA/m and resist core oxidation up to 300 °C due to the existence of a > 8 nm thin oxide passivating shell. In the second step, a composite powder is fabricated by mixing the nanowires with hexaferrite particles. After the optimal nanowire diameter and composite composition are selected, a bonded magnet is produced. The resulting magnet presents a 20% increase in remanence and an enhancement of the energy product of 48% with respect to a pure hexaferrite (strontium ferrite) magnet. These results put nanowire-ferrite composites at the forefront as candidate materials for alternative magnets for substitution of rare earths in applications that operate with moderate magnet performance.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Tuning the Néel temperature in an antiferromagnet: the case of NixCo1-xO microstructures
Authors:
Anna Mandziak,
Guiomar D. Soria,
José Emilio Prieto,
Pilar Prieto,
Cecilia Granados-Miralles,
Adrian Quesada,
Michael Foerster,
Lucia Aballe,
Juan de la Figuera
Abstract:
We show that it is possible to tune the Néel temperature of nickel(II)-cobalt(II) oxide films by changing the Ni to Co ratio. We grow single crystalline micrometric triangular islands with tens of nanometers thickness on a Ru(0001) substrate using high temperature oxygen-assisted molecular beam epitaxy. Composition is controlled by adjusting the deposition rates of Co and Ni. The morphology, shape…
▽ More
We show that it is possible to tune the Néel temperature of nickel(II)-cobalt(II) oxide films by changing the Ni to Co ratio. We grow single crystalline micrometric triangular islands with tens of nanometers thickness on a Ru(0001) substrate using high temperature oxygen-assisted molecular beam epitaxy. Composition is controlled by adjusting the deposition rates of Co and Ni. The morphology, shape, crystal structure and composition are determined by low-energy electron microscopy and diffraction, and synchrotron-based x-ray absorption spectromicroscopy. The antiferromagnetic order is observed by x-ray magnetic linear dichroism. Antiferromagnetic domains up to micrometer width are observed.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Hexaferrite-based permanent magnets with upper magnetic properties by cold sintering process via a non-aqueous solvent
Authors:
Aida Serrano,
Eduardo García-Martín,
Cecilia Granados-Miralles,
Giulio Gorni,
Jesús López-Sánchez,
Sandra Ruiz-Gómez,
Lucas Pérez,
Adrián Quesada,
José F. Fernández
Abstract:
The incessant technological pursuit towards a more sustainable and green future depends strongly on permanent magnets. At present, their use is widespread, making it imperative to develop new processing methods that generate highly competitive magnetic properties reducing the fabrication temperatures and costs. Herein, a novel strategy for develo** dense sintered magnets based on Sr-hexaferrites…
▽ More
The incessant technological pursuit towards a more sustainable and green future depends strongly on permanent magnets. At present, their use is widespread, making it imperative to develop new processing methods that generate highly competitive magnetic properties reducing the fabrication temperatures and costs. Herein, a novel strategy for develo** dense sintered magnets based on Sr-hexaferrites with upper functional characteristics is presented. An innovative cold sintering approach using glacial acetic acid as novelty, followed by a post-annealing at 1100 °C, achieves a densification of the ceramic magnets of 92% with respect to the theoretical density and allows controlling the particle growth. After the cold sintering process, a fraction of amorphous SrO is identified, in addition to a partial transformation to α-Fe2O3 as secondary crystalline phase. 46 wt% of SrFe12O19 remains, which is mostly recuperated after the post-thermal treatment. These findings do not significantly modify the final structure of ferrite magnets, neither at short- nor long-range order. The innovative process has a positive impact on the magnetic properties, yielding competitive ferrite magnets at lower sintering temperatures with an energy efficiency of at least 25%, which opens up a new horizon in the field of rare-earth free permanent magnets and new possibilities in other applications.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Remanence Increase in SrFe$_{12}$O$_{19}$/Fe Exchange-Decoupled Hard-Soft Composite Magnets Owing to Dipolar Interactions
Authors:
Jesús Carlos Guzmán-Mínguez,
Cecilia Granados-Miralles,
Patrick Kuntschke,
César de Julián Fernández,
Sergey Erokhin,
Dmitry Berkov,
Thomas Schliesch,
Jose Francisco Fernández,
Adrián Quesada
Abstract:
In the search for improved permanent magnets, fueled by the geostrategic and environmental issues associated with rare-earth-based magnets, magnetically hard (high anisotropy)-soft (high magnetization) composite magnets hold promise as alternative magnets that could replace modern permanent magnets, such as rare-earth-based and ceramic magnets, in certain applications. However, so far, the magneti…
▽ More
In the search for improved permanent magnets, fueled by the geostrategic and environmental issues associated with rare-earth-based magnets, magnetically hard (high anisotropy)-soft (high magnetization) composite magnets hold promise as alternative magnets that could replace modern permanent magnets, such as rare-earth-based and ceramic magnets, in certain applications. However, so far, the magnetic properties reported for hard-soft composites have been underwhelming. Here, an attempt to further understand the correlation between magnetic and microstructural properties in strontium ferrite-based composites, hard SrFe$_{12}$O$_{19}$ (SFO) ceramics with different contents of Fe particles as soft phase, both in powder and in dense injection molded magnets, is presented. In addition, the influence of soft phase particle dimension, in the nano- and micron-sized regimes, on these properties is studied. While Fe and SFO are not exchange-coupled in our magnets, a remanence that is higher than expected is measured. In fact, in composite injection molded anisotropic (magnetically oriented) magnets, remanence is improved by 2.4% with respect to a pure ferrite identical magnet. The analysis of the experimental results in combination with micromagnetic simulations allows us to establish that the type of interaction between hard and soft phases is of a dipolar nature, and is responsible for the alignment of a fraction of the soft spins with the magnetization of the hard. The mechanism unraveled in this work has implications for the development of novel hard-soft permanent magnets.
△ Less
Submitted 19 September, 2023;
originally announced September 2023.
-
Size effects in the Verwey transition of nanometer-thick micron-wide magnetite crystals
Authors:
Adolfo del Campo,
Sandra Ruiz-Gómez,
Eva M. Trapero,
Cecilia Granados-Miralles,
Adrián Quesada,
Michael Foerster,
Lucía Aballe,
José Emilio Prieto,
Juan de la Figuera
Abstract:
We have monitored the Verwey transition in micrometer-wide, nanometer-thick magnetite islands on epitaxial Ru films on Al2O3(0001) using Raman spectroscopy. The islands have been grown by high-temperature oxygen-assisted molecular beam epitaxy. Below 100 K and for thicknesses above 20 nm the Raman spectra correspond to those observed in bulk crystals and high quality thin films for the sub-Verwey…
▽ More
We have monitored the Verwey transition in micrometer-wide, nanometer-thick magnetite islands on epitaxial Ru films on Al2O3(0001) using Raman spectroscopy. The islands have been grown by high-temperature oxygen-assisted molecular beam epitaxy. Below 100 K and for thicknesses above 20 nm the Raman spectra correspond to those observed in bulk crystals and high quality thin films for the sub-Verwey magnetite structure. At room temperature the width of the cubic phase modes is similar to the best reported in bulk crystals, indicating a similar level of electron-phonon interaction. The evolution of the Raman spectra upon cooling suggests that for islands thicker than 20 nm, structural changes appear first at temperatures starting at 150 K and the Verwey transition itself takes place at around 115 K. However, islands thinner than 20 nm show a very different Raman spectra indicating that while a transition takes place, the charge order of the ultrathin islands differs markedly from their thicker counterparts
△ Less
Submitted 6 April, 2022;
originally announced April 2022.
-
Influence of the growth conditions on the magnetism of SrFe$_{12}$O$_{19}$ thin films and the behavior of Co / SrFe$_{12}$O$_{19}$ bilayers
Authors:
G. D. Soria,
J. F. Marco,
A. Mandziak,
S. Sánchez-Cortés,
M. Sánchez-Arenillas,
J. E. Prieto,
J. Dávalos,
M. Foerster,
L. Aballe,
J. López-Sánchez,
J. C. Guzmán-Mínguez,
C. Granados-Miralles,
J. de la Figuera,
A. Quesada
Abstract:
SrFe$_{12}$O$_{19}$ (SFO) films grown on Si (100) substrates by radio-frequency magnetron sputtering have been characterized in terms of composition, structural and magnetic properties by a combination of microscopy, diffraction and spectroscopy techniques. Mössbauer spectroscopy was used to determine the orientation of the films magnetization, which was found to be controlled by both the sputteri…
▽ More
SrFe$_{12}$O$_{19}$ (SFO) films grown on Si (100) substrates by radio-frequency magnetron sputtering have been characterized in terms of composition, structural and magnetic properties by a combination of microscopy, diffraction and spectroscopy techniques. Mössbauer spectroscopy was used to determine the orientation of the films magnetization, which was found to be controlled by both the sputtering power and the thickness of the films. Additionally, the coupling between the SFO films and a deposited cobalt overlayer was studied by means of synchrotron-based spectromicroscopy techniques. A structural coupling at the SFO/Co interface is suggested to account for the expetimental observations. Micromagnetic simulations were performed in order to reproduce the experimental behaviour of the system.
△ Less
Submitted 8 May, 2020; v1 submitted 19 February, 2020;
originally announced February 2020.