Influence of amorphous phase on coercivity in SmCo5-Cu nanocomposites
Authors:
Franziska Staab,
Yangyiwei Yang,
Eren Foya,
Enrico Bruder,
Benjamin Zingsem,
Esmaeil Adabifiroozjaei,
Konstantin Skokov,
Michael Farle,
Rafal E. Dunin-Borkowski,
Leopoldo Molina-Luna,
Oliver Gutfleisch,
Bai-Xiang Xu,
Karsten Durst
Abstract:
Severe plastic deformation of powder blends consisting of SmCo5-Cu results in magnetically hardened nanocomposite bulk materials. The microstructure is continuously refined with increasing torsional deformation, yet, coercivity saturates at a certain level of strain. Transmission electron microscopy (TEM) investigation of the microstructure reveals a partial amorphization of the SmCo5 phase due to…
▽ More
Severe plastic deformation of powder blends consisting of SmCo5-Cu results in magnetically hardened nanocomposite bulk materials. The microstructure is continuously refined with increasing torsional deformation, yet, coercivity saturates at a certain level of strain. Transmission electron microscopy (TEM) investigation of the microstructure reveals a partial amorphization of the SmCo5 phase due to high-pressure torsion by 20 applied rotations. In this amorphous matrix nanocrystals are embedded. The effect of these experimentally observed microstructural features on the magnetic properties are investigated by micromagnetic simulations, which show that an increasing volume fraction of nanocrystals is beneficial for higher coercivities. For a fixed volume fraction of nanocrystals the simulations reveal an increasing coercivity with decreasing the size of the nanocrystals due to increasing number of interfaces acting as pinning sites. Furthermore, our micromagnetic simulations disclose the mechanisms of the saturation and decline of magnetic hardening due to the strain induced by high-pressure torsion. The calculated coercivity fits very well to the experimentally observed coercivity of Hc=1.34 T. The knowledge can also be used to develop and provide optimization strategies from the microstructure perspective.
△ Less
Submitted 15 May, 2023;
originally announced May 2023.
-
Laser Powder Bed Fusion of anisotropic Nd-Fe-B bonded magnets utilizing an in situ mechanical alignment approach
Authors:
Kilian Schäfer,
Rafael Gitti Tortoretto Fim,
Fernando Maccari,
Tobias Braun,
Stefan Riegg,
Konstantin Skokov,
David Koch,
Enrico Bruder,
Iliya Radulov,
Carlos Henrique Ahrens,
Paulo Antônio Pereira Wendhausen,
Oliver Gutfleisch
Abstract:
Nd-Fe-B bonded magnets are an important class of permanent magnets, employed in many technological sectors. The Additive Manufacturing (AM) processes enables the fabrication of net-shape bonded magnets with complex geometries, allowing to tailor their magnetic stray field specifically for a given application. A crucial challenge to be addressed concerning AM of bonded magnets is the production of…
▽ More
Nd-Fe-B bonded magnets are an important class of permanent magnets, employed in many technological sectors. The Additive Manufacturing (AM) processes enables the fabrication of net-shape bonded magnets with complex geometries, allowing to tailor their magnetic stray field specifically for a given application. A crucial challenge to be addressed concerning AM of bonded magnets is the production of magnetically anisotropic components. The common approaches presented in the literature up to now, required a post-printing procedure or the complex integration of a magnetic field source into the AM process. Here, we present a technique to fabricate anisotropic bonded magnets via Laser Powder Bed Fusion (LPBF) by utilizing the mechanical alignment of anisotropic particles in a single step, without the need for a magnetic field source. Anisotropic bonded magnets were fabricated using a mixture of anisotropic Nd-Fe-B powder (MQA-38-14) and polyamide-12 (PA12). This magnetic powder consists of ellipsoidal particles, where the easy magnetization axis is distributed perpendicular to their longest side, which can be exploited to generate magnetic texture. Depending on the particle size used as feedstock, the degree of alignment (<cos$(θ)$>) can be tailored to a maximum of <cos$(θ)$> = 0.78. The fabricated anisotropic bonded magnets exhibited a maximum remanence of Jr = 377 mT and an energy product of (BH)max = 28.6 kJ/m3, respectively.
△ Less
Submitted 5 May, 2023; v1 submitted 4 May, 2023;
originally announced May 2023.
-
Influence of microstructure on the application of Ni-Mn-In Heusler compounds for multicaloric cooling using magnetic field and uniaxial stress
Authors:
Lukas Pfeuffer,
Adrià Gràcia-Condal,
Tino Gottschall,
David Koch,
Tom Faske,
Enrico Bruder,
Jonas Lemke,
Andreas Taubel,
Semih Ener,
Franziska Scheibel,
Karsten Durst,
Konstantin P. Skokov,
Lluís Mañosa,
Antoni Planes,
Oliver Gutfleisch
Abstract:
Novel multicaloric cooling utilizing the giant caloric response of Ni-Mn-based metamagnetic shape-memory alloys to different external stimuli such as magnetic field, uniaxial stress and hydrostatic pressure is a promising candidate for energy-efficient and environmentally-friendly refrigeration. However, the role of microstructure when several external fields are applied simultaneously or sequenti…
▽ More
Novel multicaloric cooling utilizing the giant caloric response of Ni-Mn-based metamagnetic shape-memory alloys to different external stimuli such as magnetic field, uniaxial stress and hydrostatic pressure is a promising candidate for energy-efficient and environmentally-friendly refrigeration. However, the role of microstructure when several external fields are applied simultaneously or sequentially has been scarcely discussed in literature. Here, we synthesized ternary Ni-Mn-In alloys by suction casting and arc melting and analyzed the microstructural influence on the response to magnetic fields and uniaxial stress. By combining SEM-EBSD and stress-strain data, a significant effect of texture on the stress-induced martensitic transformation is revealed. It is shown that a <001> texture can strongly reduce the critical transformation stresses. The effect of grain size on the material failure is demonstrated and its influence on the magnetic-field-induced transformation dynamics is investigated. Temperature-stress and temperature-magnetic field phase diagrams are established and single caloric performances are characterized in terms of $Δ{s_T}$ and $Δ{T_{ad}}$. The cyclic $Δ{T_{ad}}$ values are compared to the ones achieved in the multicaloric exploiting-hysteresis cycle. It turns out that a suction-cast microstructure and the combination of both stimuli enables outstanding caloric effects in moderate external fields which can significantly exceed the single caloric performances. In particular for Ni-Mn-In, the maximum cyclic effect in magnetic fields of 1.9 T is increased by more than 200 % to -4.1 K when a moderate sequential stress of 55 MPa is applied. Our results illustrate the crucial role of microstructure for multicaloric cooling using Ni-Mn-based metamagnetic shape-memory alloys.
△ Less
Submitted 9 November, 2021; v1 submitted 4 November, 2021;
originally announced November 2021.